PU integral skin foam material can be used to produce a product with dense epidermis and foam interior in one foaming process. So it is widely used for making chair handle, arm-rest, Steering wheels etc. Polyflex – ISF – 763, ISF – 764.
Specification:
Items | ISF – 763 | ISF – 764 |
---|---|---|
RATIO (P/I) | 100/45 | 100/45 – 55 |
Cream time | 17 – 23 Sec | 10 – 13 Sec |
Gel time | 38 – 48 Sec | 27 – 35 Sec |
Mould temperature (°C) | 35 – 45 | 40 – 50 |
Demould time (Min.) | 3 – 4 | 3 – 4 |
Frd (kg/m³) | 110 – 130 | 150 – 180 |
Mould foam density ( kg/m³) | 300 – 350 | 350 – 450 |
Surface hardness Shore - A | 65 – 70 | 60 – 70 |
Application | Chair handle, Arm rest | Steering wheels & others |